The FAA has issued a Special Airworthiness Information Bulletin (SAIB) to advise owners, operators and repair stations of aircraft equipped with the Rolls-Royce (formerly Allison) 250-C30, -C40 and -C47 series engines that a recent suspected unapproved parts investigation revealed that some combustion liners might have been modified with an unapproved metal alloy.

 